Todd Leon Mansfield, Cincinnati, OH.
Assigned to The Procter & Gamble Company, Cincinnati, OH.
Filed: 11/7/13
Issued: 4/12/16
A stretch laminate comprising: a first layer comprising an elastomer film having a skin, the first layer having a surface; and a second layer comprising a nonwoven material, the second layer having a basis weight of less than about 25 gsm and a surface that is attached to the surface of the first layer, the elastomer film having an engineering tensile strength, at an engineering strain rate of about 600/s, of at least one of about greater than about 14 MPa for a plain specimen or about greater than about 7 MPa for a notched specimen.
Assigned to The Procter & Gamble Company, Cincinnati, OH.
Filed: 11/7/13
Issued: 4/12/16
A stretch laminate comprising: a first layer comprising an elastomer film having a skin, the first layer having a surface; and a second layer comprising a nonwoven material, the second layer having a basis weight of less than about 25 gsm and a surface that is attached to the surface of the first layer, the elastomer film having an engineering tensile strength, at an engineering strain rate of about 600/s, of at least one of about greater than about 14 MPa for a plain specimen or about greater than about 7 MPa for a notched specimen.